在常規(guī)法X射線應(yīng)力測定中,對衍射線的強度校正,不論在背底部分,還是在純衍射線部分,吸收校正是本質(zhì)的校正。在許多工程測量中,只進行吸收校正,就可以達(dá)到足夠的準(zhǔn)確度,以此為根據(jù),本文提出一種可在連續(xù)掃描測量中進行強度校正的方法:利用在透明膠片上預(yù)先繪制的吸收曲線來擬合背底,同時進行定峰,采用這種方法可以較好地進行背底扣除,也對純衍射線的強度做了吸收校正。試驗結(jié)果說明這種方法是可靠的。
A set of absorption curves was priorly prepared on transparent films to fit thebackground and peak intensities in continuous scanning X-ray stress measurement. It may bebetter to correct both background and absorption of pure diffraction intensity. Experimentalresults revealed this to be a reliable correction method.
文獻(xiàn)名稱 |
一種連續(xù)掃描X射線應(yīng)力測定的強度校正方法 |
Article Name |
A METHOD FOR CORRECTING INTENSITY IN CONTINUOUS SCANNING X-RAY STRESS MEASUREMENT; |
作者 |
李家寶; 康增橋; 何家文; |
Author |
LI Jiabao;KANG Zengqiao;HE Jiawen National Laboratory for Fatigue and Fracture of Materials;Institute of Metal Research;Academia Sinica;Shenyang;Xi'an Jiaotong University Correspondent;associate professor;Shenyang 110015; |
作者單位 |
中國科學(xué)院金屬研究所; 材料疲勞與斷裂國家重點實驗室; 西安交通大學(xué) 副研究員; 沈陽(110015)中國科學(xué)院金屬研究所; |
文獻(xiàn)出處 |
金屬學(xué)報;Acta Metallrugica Sinica;1992年 05期; |
關(guān)鍵詞 |
X射線衍射; 應(yīng)力測定; 強度校正; 定峰; |
Keywords |
X-ray diffraction;stress measurement;intensity correction;peak location |